| Product |
Liner |
Carrier |
Thickness mm |
Adhesive |
Service Temp. ¢J |
Features / Applications |
| C201 |
130g/m2 PE laminated Kraft paper |
Unsupported |
0.035 |
Electric Conductive Acrylic |
-20 ~ 100 |
Main applications :
a) Lamination to electronic parts and components for removing static and thus preventing electric shock.
b) When laminated to copper foil, forms an excellent electromagnetic shielding material. |
| K203 |
80 g/m2 white Glassine paper |
Unsupported |
0.045 |
Acrylic |
-20 ~ 120 |
Excellent tacky and good shear strength for immediate bonding purpose.
Good resistance to solvent, heat and chemical. |
| W203 |
130g/m2 PE laminated Kraft paper |
Unsupported |
0.05 |
Acrylic |
-20 ~100 |
Good temperature and chemical resistance.
Long term bonding results with most substrates ¡V metal, plastic and high-energy surfaces.
Suitable for applications on relative smooth surfaces. |
| W204 |
130g/m2 PE laminated Kraft paper |
Unsupported |
0.05 |
Acrylic |
-40 ~ 200 |
High temperature, chemical and water permeation resistance.
Long term bonding for general purpose applications.
Suitable for applications on relatively smooth surfaces. |
| W205 |
130g/m2 PE laminated Kraft paper |
Unsupported |
0.038 |
Acrylic |
-20 ~ 100 |
General purpose applications. |
| W207 |
130g/m2 PE laminated Kraft paper |
Unsupported |
0.06 |
Acrylic |
-40 ~ 90 |
Good temperature and chemical resistance.
Good bonding effects to low energy surface and extreme environment conditions. |
| ¡¸W208 |
130g/m2 PE laminated Kraft paper |
Unsupported |
0.06 |
White Acrylic |
-40 ~ 120 |
¡¸Flame retardant adhesive, UL94-V0 approved item.
Long term bonding for flame retardant applications.(PICTURE) |
| W209 |
130g/m2 PE laminated Kraft paper |
Unsupported |
0.04 |
Acrylic |
-40 ~ 100 |
Exceptional temperature and chemical resistance.
Long term bonding results with most substrates ¡V metal, plastic and high-energy surfaces, especially in low temperature and extreme environment conditions. |
| HA206 |
130g/m2 PE laminated Kraft paper |
Unsupported |
0.06 |
Heat Activated |
-20 ~ 120 |
Bonding film with pressure heat activated at temperature 150¢J, which by thermal bonding forms a durable, long lasting bond to most EVA, EPDM, PU, and PP-based plastic materials. |
| Y207 |
90 g/m2 Havana Glassine paper |
Unsupported |
0.1 |
Acrylic |
-40 ~ 100 |
Good temperature and chemical resistance.
Good bonding effect to low energy and porous surfaces and extreme environment conditions.